Index: 35470-70853

Drizoro - malta pro vyplňování spár Maxjoint PAV

Average grade: 0 / 0 reviews
Mortar based on cement, silica and special additives, which when mixed with water forms a liquid product, characterized by high mechanical strength and shrinkage compensating properties. It is used to fill joints of internal and external pavements.

kolor

Save amount -
57,81 zł 57,81 zł
S DPH

Najniższa cena z ostatnich 30 dni: 57,81 zł brutto. (47,00 zł)

On product inquiry
cennikowa cena jednostkowa netto
4,94 zł
za kg
cennikowa cena jednostkowa brutto
6,08 zł
za kg
promocyjna cena jednostkowa netto
4,70 zł
za kg
promocyjna cena jednostkowa brutto
5,78 zł
za kg
całkowita cena cennikowa netto
49,40 zł
za 10 kg
całkowita cena cennikowa brutto
60,76 zł
za 10 kg
całkowita cena cennikowa netto
47,00 zł
za 10 kg
całkowita cena cennikowa brutto
57,81 zł
za 10 kg

Products description

Mortar based on cement, silica and special additives, which when mixed with water forms a liquid product, characterized by high mechanical strength and shrinkage compensating properties. It is used to fill joints of internal and external pavements.

Features

  • high mechanical strength
  • shrinkage compensation does not introduce stresses at setting and does not delaminate
  • the high viscosity of the fresh mortar prevents sedimentation
  • high resistance to fat and oil
  • does not contain chloride or metal particles
  • high fluidity allowing for quick and easy placement
  • very good adhesion to the substrate

Application

  • filling of joints in floors, roof with natural stone
  • surfaces exposed to pedestrian and vehicle traffic
  • filling paving stones in gardens, public paths, squares, etc.

Technical data

  • appearance of gray or white powder
  • aggregate size 0–2 mm
  • powder density 1.28 0.05 g / cm 3
  • conditions of application and maturation - mixing water 12-14%
  • no sedimentation of fresh mortar
  • setting time at 20 C 6-7 h
  • maturing time for pedestrian traffic 20 C 24/48 h
  • the density of the hardened mortar 2.25 0.05 g / cm 3
  • compressive strength 24 h - 25.0 MPa; 7 days - 52.5 MPa; 28 days - 71.0 MPa
  • bending strength 24 h - 3.5 MPa; 7 days - 8.1 MPa; 28 days - 10.2 MPa
  • approximate consumption 2.0 kg / m 2 / mm